Quality 1.6772

General Product Description

Material number 1.6772

Short name according to EN 1.6772

Applicable standards KTA 3201.1, VdTÜV-Blatt 337

Treatment quneched and tempered

Variations

QualityTreatmentShapeDimension (mm)
1.6772quneched and temperedRoundRound24,83 + 30,5
Your inquiry

Description

Connecting parts, mechanical engineering

Chemical composition (in %)

CCrNiMoAlMnSiPS
Min 0,18 1,20 3,4 0,25 0,005 0,30 0,15 - -
Max 0,25 1,50 4,0 0,50 0,050 0,50 0,40 0,02 0,01
ElementMinMax
C 0,18 0,25
Cr 1,20 1,50
Ni 3,4 4,0
Mo 0,25 0,50
Al 0,005 0,050
Mn 0,30 0,50
Si 0,15 0,40
P - 0,02
S - 0,01

Mechanical properties (quenching and tempering)

Tensile strength Rm 1040–1240 N/mm2

0.2% proof stress Rp0.2 980 (705 bei 400°C) N/mm2

Elongation at break A5 14 %

Notched impact energy (ISO-V) ~75 (~31 bei -40°C) J

Magnetizability Yes

Typical areas of application

connectors

Mechanical engineering

highly stressed components

General properties (quenching and tempering)

Corrosion Resistance

Weldability

Forgeability

Tensionability

= Low
= Very Good

Note

All information in this data sheet has been compiled to the best of our knowledge and belief. It is for information purposes only and does not constitute a assured property or guarantee. For the suitability of the material in specific applications, we recommend carrying out appropriate inspections and tests. Any liability for damage or errors is excluded.